superalloys/high temperature alloy parts manufacturer,inconel718
superalloys/high temperature alloy parts manufacturer,inconel718

Artisan Industry

Superalloy Parts Supplier

  • HOME
  • About Us
  • Products 
    • superalloys fasteners
    • Aerospace Fittings
    • Energy Power
    • Petrochemical
    • Gas Turbine
    • Sputtering Targets
    • Stainless steel Fabrication
  • Factory Capacity 
    • Research & Design
    • Vacuum Investment Casting
    • Precision Forging
    • CNC Machining
    • Quality Control
    • Documents Download
  • Technical Support
  • …  
    • HOME
    • About Us
    • Products 
      • superalloys fasteners
      • Aerospace Fittings
      • Energy Power
      • Petrochemical
      • Gas Turbine
      • Sputtering Targets
      • Stainless steel Fabrication
    • Factory Capacity 
      • Research & Design
      • Vacuum Investment Casting
      • Precision Forging
      • CNC Machining
      • Quality Control
      • Documents Download
    • Technical Support
Get Instant Price
superalloys/high temperature alloy parts manufacturer,inconel718
superalloys/high temperature alloy parts manufacturer,inconel718

Artisan Industry

Superalloy Parts Supplier

  • HOME
  • About Us
  • Products 
    • superalloys fasteners
    • Aerospace Fittings
    • Energy Power
    • Petrochemical
    • Gas Turbine
    • Sputtering Targets
    • Stainless steel Fabrication
  • Factory Capacity 
    • Research & Design
    • Vacuum Investment Casting
    • Precision Forging
    • CNC Machining
    • Quality Control
    • Documents Download
  • Technical Support
  • …  
    • HOME
    • About Us
    • Products 
      • superalloys fasteners
      • Aerospace Fittings
      • Energy Power
      • Petrochemical
      • Gas Turbine
      • Sputtering Targets
      • Stainless steel Fabrication
    • Factory Capacity 
      • Research & Design
      • Vacuum Investment Casting
      • Precision Forging
      • CNC Machining
      • Quality Control
      • Documents Download
    • Technical Support
Get Instant Price
superalloys/high temperature alloy parts manufacturer,inconel718

Aerospace Fasteners :HASTELLOY C-276

Superalloy parts Manufacturer & supplier .Including Impeller/Turbine/Firebox/Combustor

APPLICATIONS OF HASTELLOY C-276

  • Bellows
  • Marine hardware
  • Chemical processing
  • Agrichemical production
  • Petrochemical production
  • Aerospace Fasteners

DESCRIPTION OF HASTELLOY C-276

Hastelloy® C-276 is a very versatile nickel-molybdenum-chromium-tungsten alloy with excellent corrosion resistance and good fabricability. While it does have good oxidation resistance up to 1800°F, Hastelloy alloy C-276 is generally not recommended for elevated temperature service.

Nickel Alloy C-276 has resisted the formation of grain boundary precipitates in the weld-heat affected zone, making it a candidate for most chemical and petrochemical processing applications in the as-welded condition. HC276 is a nickel alloy that is has excellent resistance to reducing acids, sulfuric acid, hydrochloric acid, brine solutions, oxidizing chlorides, and hot seawater.

Hastelloy C-276 is also one of the few materials resistant to wet chlorine gas, hypochlorite and chlorine dioxide. This particular nickel alloy has exceptional resistance to crevice corrosion and stress corrosion cracking, as well as chloride pitting. It's low carbon content minimizes carbide precipitation during welding preserves its excellent resistance to corrosion during welding. This translates to C-276 being readily fabricated by welding using methods similar to those utilized for nickel-based alloys.

Hastelloy C-276 is also known as:

  • Nickel C-276
  • Alloy C-276
  • Inconel C-276

WHAT ARE THE PHYSICAL PROPERTIES OF HASTELLOY C-276?

Density: 0.321 lbs/in3, 8.89 g/cm3
Mean Coefficient of Thermal Expansion: in/in/° F (mm/m/ °C):
70 - 212 °F (20 - 100 ° C): 6.2 x 10-5 (11.2)

Thermal Conductivity: BTU-in/h-ft-°F (W/m-°K):
70 °F (21 °C): 71 (10.2)

Modulus of Elasticity: ksi (MPa)
29.8 x 103 (205 x 103) in tension
Melting Point: 2500 °F (1371 °C)

HASTELLOY FORMS SUPPLIED BY ULBRICH

  • Hastelloy C-276 Coils
  • Hastelloy C-276 Strip
  • Hastelloy C-276 Foil
  • Hastelloy C-276 Ribbon
  • Hastelloy C-276 Wire Profiles
  • Hastelloy C-276 Shaped Wire Profiles
  • Hastelloy C-276 Round Wire
  • Hastelloy C-276 Flat Wire
  • Hastelloy C-276 Square Wire

MECHANICAL PROPERTIES AT ROOM TEMPERATURE

ANNEALED PROPERTIES OF HASTELLOY C-276

Ultimate Tensile Strength: 100 KSI min (690 MPa min)
Yield Strength: (0.2% offset) 45 KSI min (31 0 MPa min)
Elongation: 40% min
Hardness: Rb 100 min (aim)

TEMPERED:

Hastelloy® C-276 can be cold rolled to various tempers. Contact Ulbrich Technical Service for additional information.

ADDITIONAL PROPERTIES

HASTELLOY C-276 CORROSION RESISTANCE DATA

HASTELLOY C-276 is a nickel-chromium-molybdenum alloy with universal corrosion resistance unmatched by any other alloy. It has outstanding resistance to a wide variety of chemical process environments including hot contaminated mineral acids, ferric and cupric chlorides,solvents, chlorine and chlorine contaminated (both organic and inorganic), dry chlorine, acetic anhydride, formic and acetic acids, sea water and brine solutions, chlorine dioxide solutions, and hypochlorite.

AVAILABLE FINISHES FOR HASTELLOY C276

1、Hot rolled annealed and descaled. It is available in strip, foil and ribbon. It is used for applications where a smooth decorative finish is not required.
2、Dull finish produced by cold rolling, annealing and descaling. Used for deep drawn parts and those parts that need to retain lubricants in the forming process.
3、Smooth finish produced by cold rolling, annealing and descaling. A light cold rolling pass is added after anneal with polished rolls giving it a brighter finish than 4、CBACourse bright annealed cold rolled matte finish and bright anneal
5、Smooth finish produced by cold rolling and bright annealing. A light pass using highly polished rolls produces a glossy finish. A 2BA finish may be used for lightly formed applications where a glossy finish is desired in the formed part
* Not all finishes are available in all alloys - Contact Ulbrich Sales for more information.

WIRE FINISHES FOR HASTELLOY C-276

XCExtra Clean Bright Annealed or Bright Annealed and Cold Rolled Grease - Ultra bright finish (for decorative applications) Soap - Soap coating on tempered wire to act as lubricant.
SuperFinish™ is an extra clean extra smooth polished finish available only at Ulbrich

* Contact Ulbrich Wire for custom wire finishes.

HEAT TREATMENT

Hastelloy® C-276 cannot be hardened heat treating.

WELDING

For best results refer to: SSINA's "Welding of Stainless Steels and Other Joining Methods"

Hastelloy® C-276 is a grade of Hastelloy® which is a nickel-molybdenum alloy. There are many different grades of Hastelloy®, which includes C-276. Grades of Hastelloy® have each been optimized for a specific purpose. Molybdenum makes Hastelloy® harder and stronger at high temperatures. This alloying element and the characteristics it imbues into the material also makes it great for welding applications. These nickel alloys are easily fabricated and formed. They also exhibit good ductility and are able to be cold worked.

All grades of Hastelloy® are considered to be a corrosion resistant alloy because each grade exhibits superior resistance to various corrosive environments. Hastelloy® has outstanding resistance to highly oxidizing corrosives such as oxidizing salts and reducing agents, making it a great alloy to specify for applications used in moderate to severe corrosive environments.

Limitation of Liability and Disclaimer of Warranty: In no event will Ulbrich Stainless Steels & Special Metals, Inc., be liable for any damages arising from the use of the information included in this document or that it is suitable for the 'applications' noted. We believe the information and data provided to be accurate to the best of our knowledge but, all data is considered typical values only. It is intended for reference and general information and not recommended for specification, design or engineering purposes. Ulbrich assumes no implied or express warranty in regard to the creation or accuracy of the data provided in this document.

Artison is a supplier of aerospace components; Products include impeller, turbine, combustion chamber, fastener, etc.

If you have any questions or needs, please contact us. Here is our contact information:

Price Inquiry:sales.lily@superalloyparts.com 

Technical Support:eng.daisy@superalloyparts.com 

Quality Control:qc.jason@superalloyparts.com

 

Subscribe
Previous
Aerospace parts :Impller
Next
Anti-wear Of Impeller/Supplier of Superalloy Parts...
 Return to site
Profile picture
Cancel
Cookie Use
We use cookies to improve browsing experience, security, and data collection. By accepting, you agree to the use of cookies for advertising and analytics. You can change your cookie settings at any time. Learn More
Accept all
Settings
Decline All
Cookie Settings
These cookies enable core functionality such as security, network management, and accessibility. These cookies can’t be switched off.
These cookies help us better understand how visitors interact with our website and help us discover errors.
These cookies allow the website to remember choices you've made to provide enhanced functionality and personalization.
Save