Deliver Fast/accelerated delivery/Fasteners Manufacturers MP35N Nickel Cobalt Alloy Metric Hex Head Bolts Screws,Nickel MP35N UNS R30035 High Performance Alloy bolts supplier,MP35N fasteners owe their extraordinary strength to a unique alloy combination of nickel, cobalt, chrome and molybdenum and have ultimate tensile strengths.
Mp35n Bolts and UNS R30035 Screws/ Studs

September 29, 2025

Of course. Here is a detailed introduction to MP35N fasteners, covering their composition, key properties, manufacturing process, applications, and a comparison with other high-performance alloys.

Introduction to MP35N Fasteners

MP35N is a premium-grade, multi-phase cobalt-chromium-nickel-molybdenum alloy renowned for its unique combination of ultimate strength, exceptional corrosion resistance, and high toughness. It is not a single-phase material but derives its properties from a specialized thermomechanical processing technique.

The name "MP35N" stands for "Multi-Phase, 35% Nickel." It is often considered the "gold standard" for fasteners in the most demanding applications where failure is not an option.

1. Key Characteristics and Properties

MP35N fasteners excel due to a suite of outstanding properties:

  • Ultra-High Strength: The most notable feature is its ability to achieve tensile strengths exceeding 300 ksi (2,070 MPa) and yield strengths over 260 ksi (1,790 MPa), which is significantly higher than many other high-strength alloys.

  • Exceptional Corrosion Resistance: It exhibits virtually complete resistance to chloride-ion stress corrosion cracking (SCC) and outstanding performance in sour (H₂S) environments, seawater, and other aggressive chemical media.

  • High Fatigue Strength: Its resistance to crack propagation makes it excellent for applications subject to dynamic and cyclic loading.

  • Excellent Fracture Toughness: Unlike some very high-strength steels that can become brittle, MP35N maintains good ductility and toughness even at its highest strength levels.

  • Biocompatibility: In its wrought, annealed condition, MP35N is biocompatible, making it suitable for surgical implants and medical devices.

2. The Secret: Composition and Strengthening Mechanism

The extraordinary properties of MP35N are a direct result of its chemistry and processing.

  • Nominal Composition:

    • Cobalt (Co): 35% - Provides solid solution strengthening and stability at high temperatures.

    • Nickel (Ni): 35% - Stabilizes the face-centered cubic (FCC) austenitic phase and enhances corrosion resistance.

    • Chromium (Cr): 20% - Imparts outstanding corrosion resistance by forming a protective passive oxide layer.

    • Molybdenum (Mo): 10% - Enhances strength and resistance to pitting and crevice corrosion.

  • Strengthening Mechanism - Thermomechanical Processing:
    This is the core of what makes MP35N special. The alloy is strengthened not by traditional martensitic transformation (like steel) but by a "cold work and age" process.

    1. Solution Annealing: The material is first heated to a high temperature to form a single, soft, Face-Centered Cubic (FCC) phase.

    2. Severe Cold Working: The material is then heavily cold-worked (e.g., cold drawn, rolled, or forged). This deformation introduces a high density of dislocations and strains the crystal structure, significantly increasing its strength.

    3. Aging Heat Treatment: The cold-worked material is heated to an intermediate temperature (~500-650°C). This aging step prompts a controlled transformation from the FCC phase to a fine, intimate mixture of a hexagonal close-packed (HCP) phase within the FCC matrix. This multi-phase (FCC + HCP) nanostructure creates immense obstacles to dislocation movement, resulting in a dramatic increase in strength without a significant loss of toughness.

3. Manufacturing of MP35N Fasteners

Producing MP35N fasteners is a challenging and specialized process:

  1. Wire Drawing: The alloy rod is cold-drawn through a series of dies to reduce its diameter and achieve the desired level of cold work.

  2. Heading: The cold-worked wire is then cut and formed into the shape of the fastener (bolt head, screw thread) using high-pressure headers. This is a difficult process due to the material's high strength and work-hardening rate.

  3. Thread Rolling: Threads are formed by rolling rather than cutting. This cold-works the thread roots, improving fatigue strength and avoiding the creation of stress concentrations from machining.

  4. Aging Heat Treatment: The finished fastener undergoes the precise aging treatment to achieve its final ultra-high strength properties.

  5. Quality Control: Each batch undergoes rigorous testing, including tensile testing, hardness checks, and microstructural analysis, to ensure it meets stringent specifications like ASTM F562 (for wrought alloy) or AMS 5844.

4. Common Applications

MP35N fasteners are used where extreme reliability is paramount, justifying their high cost.

  • Aerospace & Defense:

    • Jet engine components (bolts, studs)

    • Airframe structural components

    • Landing gear systems

    • Missile and rocket systems

  • Oil & Gas (Downhole Tools):

    • Fasteners for equipment in deep, sour wells with high H₂S and chloride content.

    • Subsea equipment and connectors.

  • Medical Devices:

    • Bone screws, orthopedic cables, and fracture fixation plates.

    • Components in pacemakers and other implantable devices.

  • Marine & Chemical Processing:

    • Fasteners for use in seawater desalination plants and highly corrosive chemical environments

5. Comparison with Other High-Performance Alloys

Property / AlloyMP35NInconel 718A286 (Stainless)Ti-6Al-4V
Max StrengthVery High (300+ ksi)High (220 ksi)Medium-High (140 ksi)High (160-180 ksi)
Corrosion ResistanceExcellent (Best in class vs. SCC)ExcellentGoodExcellent (but different)
DensityHigh (~8.4 g/cm³)High (~8.2 g/cm³)High (~7.9 g/cm³)Low (~4.4 g/cm³)
Temperature LimitGood (up to ~650°F / 340°C)Excellent (up to ~1300°F / 700°C)Good (up to ~1300°F / 700°C)Good (up to ~800°F / 430°C)
Primary AdvantageStrength + Corrosion ResistanceHigh-Temp StrengthCost-Effective for moderate tempsStrength-to-Weight Ratio
CostVery HighHighModerateHigh

Summary of Advantages and Disadvantages

Advantages:

  • Unmatched combination of strength, toughness, and corrosion resistance.

  • Superior resistance to stress corrosion cracking (SCC) and hydrogen embrittlement.

  • Excellent fatigue performance.

  • Biocompatible for medical use.

Disadvantages:

  • Extremely high cost (one of the most expensive fastener materials).

  • Difficult to machine and form, requiring specialized tooling and processes.

  • High density is a disadvantage for weight-critical applications compared to titanium.

  • Not a high-temperature alloy like Inconel 718; its strength drops off significantly above ~650°F (340°C).

In conclusion, MP35N fasteners are engineered for the most critical applications where the consequences of failure are severe. Their unique thermomechanical processing creates a material that pushes the boundaries of what is possible for a metallic fastener, making them the material of choice in the harshest environments of aerospace, medicine, and energy extraction.